A213 310H Stainless Steel Boiler Tube
A213 TP310H Stainless Steel Cold Drawn Tube is manufactured using high-quality raw materials from reliable and trusted suppliers in the industry. These products undergo various heat treatments and testing procedures such as impact test, hydrostatic test, tensile test and non-destructive electrical test to verify that they meet the specified properties.
A213 310H grade is also known as UNS S31009 grade. A213 310H high temperature stainless steel pipe is an improved version developed by increasing carbon content to enhance creep resistance. Like other austenitic grades, A213 310H boiler tube also has high nickel and chromium content and excellent toughness, even at low temperatures, although other grades are usually used in sub-zero environments.
And A213 TP310H seamless boiler tube has good resistance to thermal fatigue and cyclic heating. It can be used up to 1040 degree for intermittent use and 1150 degree for continuous use.
Specification of A213 SS TP310H Seamless Tubes
| ASTM A213 / ASME SA213 | |
| 1/2" OD - 12" OD | |
| 3.00 mm - 219.10 mm, 6.35 mm O.D to 114.3 mm O.D | |
| {{0}}.40 mm - 12.70 mm, 0.8 mm to12.7 mm | |
| SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH120, SCH140, SCH160, XXS | |
A213 310H seamless steel pipe

Gnee has 14 steel production lines, 10 processing equipment for processing, bending, painting, heat treatment, cutting, drilling, beveling, tempering, surface treatment, complete testing equipment and strong technical force. The annual production capacity is more than 60,000 tons.

1.Q.What's your advantage?
2.Q.Can your products be customized?
3.Q. Do you have a quality control system?
Populāri tagi: a213 310h stainless steel boiler tube, China a213 310h stainless steel boiler tube manufacturers, suppliers, factory